Atomic Layer Deposition is a deposition technique for very thin layers with the thickness control down to a single atomic layer. It belongs to the CVD techniques family. The thickness precision is achieved by pulsed deposition, where first a metal-containing precursor is introduced into the chamber and after a short time (allowing for a monolayer adsorption) the chamber is pumped down. Following step is an exposure to the oxidizing precursor (for oxides) or nitrogen containing precursor (for nitrides). Thus, a monolayer of target material is grown. The metal-containing precursors are usually organometallic ones, for oxidation a water or oxygen plasma can be used, nitridation is done using water or nitrogen plasma. To achieve the deposition in the ALD mode, sample is heated up to a certain temperature, for most processes being in the range from 150 to 300 °C.
| thermal deposition within range RT-500 °C | |
|---|---|
| sample size up to 8" | |
| 4 precursor lines, with possible upgrade to 6 | |
| plasma enhanced deposition (4 plasma gas lines) | |
| expo mode for homogenous deposition on high-aspect-ratio nanostructures | |
| controling software allows preparation/modification/storage of individual recipes | |
| fully automatic programmable operation | |
| Standard materials | La2O3, Al2O3, HfO2, TiO2, SiO2 |